Influence of aesthetic coating on the load-deflection ratio of nickel–titanium archwires
Aim: To assess the influence of aesthetic surface coating on load-deflection ratios in nickel-titanium (NiTi) orthodontic wires compared with uncoated wires.Methods: NiTi wires (0.016") from four different manufacturers (Morelli, Sorocaba, SP, Brazil; TP, La Porte, IN, USA; Eurodonto, Curitiba...