MACHINING PROPETIES OF COCONUT PALM WOOD

Kiln dried coconut lumber with 16 percent average moisture content were subjected to five common wood working processes composed of planing, boring, shaping, turning and sanding. Tungsten carbide cutters were used in each process except in sanding where silicon no. 60 sandpaper was employed. The coc...