Synthesis and properties of 0.3%Y2O3/0.3%La2O3/0.3%Al2O3/Cu composite

The 0.3%Y2O3/0.3%La2O3/0.3%Al2O3/Cu composite was prepared by oxygen and nitrogen atomization spray deposition technique, internal oxidation, and then treated by annealing at different temperatures. Physical properties such as microstructures, fracture appearance, hardness, strength, electrical cond...