Microstructural Evolution and Creep Behavior of the Weld Interface between 10% Cr Steel and Haynes 282 Filler Metal
This study investigated the microstructural evolution of the weld interface and creep fracture behavior of 10% Cr martensitic steel welds using Haynes 282 filler metal. The welded joints were subjected to post-weld heat treatment (PWHT) at temperatures of 738 °C for 4, 8, and 15 h. Creep tests were...