High Temperature Oxidation and Wear Behaviors of Ti–V–Cr Fireproof Titanium Alloy

The high temperature oxidation and wear behaviors of Ti–35V–15Cr–0.3Si–0.1C fireproof titanium alloy were examined at 873 and 1073 K. The oxidation weight gain after oxidation at 1073 K for 100 h was significantly larger than that at 873 K. Based on the analyses of the oxidation reaction index and o...