Microstructural Investigation of W-Cu Composite and 1Cr18Ni9 Stainless Steel Brazed Joint with Ag-Cu Filler Metal

Abstract: Tungsten-copper (W-Cu) composite and 1Cr18Ni9 stainless steel were brazed with Ag-28wt%Cu brazing filler metal in a vacuum furnace, via controlling brazing temperature 855–865 °C and holding time 30 min. Microstructure, microhardness, four-point bend strength, element distribution and phas...

Full description

Bibliographic Details
Main Authors: Xia C. Z., Liang Q. H., Zou J. S., Xu X. P.
Format: Article
Language:English
Published: De Gruyter 2014-06-01
Series:High Temperature Materials and Processes
Subjects:
Online Access:https://doi.org/10.1515/htmp-2013-0062