Samples of the ionomer glass known as G338 have been heated at 240°C for 24 hours, after which they lost 1.19 % (Standard deviation 0.16%) of their original mass. This loss was attributed to removal of water, as both molecular water and the product of reaction of silanol groups to form siloxane bri...