Chemical Bath Deposition Derived Transparent Conductive Oxide ZnO Thin Films and Their Property Characterization

碩士 === 逢甲大學 === 材料科學所 === 95 === Zinc oxide thin films were synthesized on the glass substrates via a simple, low-temperature wet chemical process—chemical bath deposition (CBD) technique with operating temperature at 60~75oC, deposition time ranging from 30 min to 180 min. The deposited films were...