The study of Heat-treatment Distortion on SKD11 and DC53
碩士 === 國立高雄第一科技大學 === 機械與自動化工程所 === 97 === Typical cold work die materials exhibit high hardness and toughness, secondary hardening, excellent wear resistance properties. Two kinds of cold work die steel, such as SKD11 and DC53, were separately quenched at 1000℃, 1025℃, and 1050 ℃, then tempered at...