Study of Repair Welding of Damaged HP Alloy Furnace Pipes

碩士 === 長庚大學 === 機械工程學系 === 104 === Nickel-based HP alloys have good weldability and outstanding resistance in corrosion, oxidation and carburization. HP alloys have been widely used in petrochemical industry for facility operated between 800℃ to 1000℃ due to their specially designed compositions and...