In-situ Reduction by Incorporating H2 Filled Hollow Glass Microspheres in PM HIP Capsules

For many metal components the presence of hard, non-metallic inclusions such as oxides lowers the impact toughness by acting as fracture initiation points and easing crack propagation. In components produced by powder metallurgy hot isostatic pressing (PM HIP), oxides often form a continuous network...