The effect of moisture exposure on pretreated aluminum alloys

Changes in pretreated 5182, 6061 and 7075 aluminum surfaces on exposure to moisture for short times was studied. The pretreatment used was the standard ASTM method for FPL etching of aluminum. The moisture treatment used was either immersion in water at 81° C or exposure to water vapor at 81° C. The...