Phase and Morphological Studies of LiCo0.3Ni0.3Mn0.3Ti0.1-xSnxO2 Cathode Materials
The substitution of LiCo0.3Ni0.3Mn0.3Ti0.1O2 materials with Sn is done to investigate the effect on the phase and morphology. The materials were synthesized via a combustion method. The annealing temperature and time of the precursors was obtained at 700 °C for 24 hours. The crystalline phase and pu...